Dew Point Corrosion in Flue Gas Heat Exchangers: Causes, Process and Prevention
Categories

How Dew Point Corrosion Develops in Flue Gas Heat Exchangers

Dew point corrosion in flue gas heat exchangers does not occur suddenly. It develops through a predictable sequence involving sulfur compounds, water vapor, low wall temperature, acidic condensate, ash deposits, and localized metal attack.
Nov 18th,2026 35 Views
Catalog

How Dew Point Corrosion Develops in Flue Gas Heat Exchangers

Dew point corrosion in flue gas heat exchangers does not occur suddenly. It develops through a predictable sequence involving sulfur compounds, water vapor, low wall temperature, acidic condensate, ash deposits, and localized metal attack.

For finned tube heat exchanger manufacturers, understanding this mechanism is essential for designing reliable air preheaters, economizers, waste heat recovery units, gas coolers, and boiler heat exchanger systems.

What Is Dew Point Corrosion?

Dew point corrosion is a low-temperature corrosion process caused by acidic condensate forming on heat exchanger tube surfaces. In sulfur-containing flue gas, the most damaging condensate is usually sulfuric acid.

Unlike ordinary water condensation, acid condensation can begin at much higher temperatures. This is why a flue gas heat exchanger may corrode even when its metal surface temperature is far above the normal water dew point.

Step 1: SO₃ Reacts with Water Vapor

When sulfur-containing fuel is burned, most sulfur is converted into sulfur dioxide (SO₂). A smaller portion, typically around 1% to 3%, is further oxidized into sulfur trioxide (SO₃).

The SO₃ combines with water vapor in the flue gas and forms sulfuric acid vapor. This reaction raises the acid dew point significantly.

Flue Gas Component or Condition Typical Effect on Dew Point Corrosion
Sulfur in fuel Increases SO₂ and SO₃ generation
SO₂ Main sulfur combustion product
SO₃ Key precursor of sulfuric acid vapor
Water vapor Combines with SO₃ to form acid vapor
Water dew point Usually about 40–50°C
Acid dew point in sulfur-bearing flue gas Commonly about 120–150°C
Higher SO₃ concentration Raises acid dew point and corrosion risk

Because the acid dew point can reach 120–150°C, the cold-end section of a flue gas heat exchanger is particularly vulnerable.

Step 2: Tube Wall Temperature Falls Below the Acid Dew Point

Once the finned tube wall temperature drops below the acid dew point, sulfuric acid vapor starts to condense on the metal surface.

The lower the wall temperature, the more acidic liquid forms. At the same time, the corrosion rate increases quickly.

In practical operation:

  • When wall temperature is only slightly below the acid dew point, corrosion may remain relatively slow.
  • When wall temperature is 10°C below the dew point, the risk begins to rise.
  • When wall temperature is 20–30°C below the dew point, acid condensation and corrosion can accelerate sharply.

This is why heat exchanger design should focus on minimum metal wall temperature, not only on average flue gas outlet temperature.

Step 3: Acid Condensate Captures Fly Ash and Forms Deposits

After sulfuric acid condenses on the tube surface, it attracts and bonds with fly ash in the flue gas. Over time, an acidic ash deposit or fouling layer develops.

This deposit layer creates several problems at once:

  1. It traps acidic moisture against the finned tube surface.
  2. It causes under-deposit corrosion.
  3. It reduces heat transfer efficiency.
  4. It increases pressure drop across the heat exchanger.
  5. It lowers the local metal temperature even further.

The result is a self-reinforcing cycle:

acid condensation → ash adhesion → fouling → reduced heat transfer → lower wall temperature → more acid condensation

For finned tube heat exchangers, this cycle is especially important because fin roots, narrow fin spacing, and poorly cleaned areas can retain deposits more easily.

Step 4: Localized Corrosion Causes Leakage and Failure

Dew point corrosion is usually not uniform across the entire heat exchanger. It often starts in localized high-risk areas, including:

  • Weld seams
  • Fin roots
  • Tube ends
  • Tube-to-tube-sheet connections
  • Cold-end tube bundles
  • Areas with poor gas distribution
  • Areas with low water flow or low inlet water temperature

As a result, the heat exchanger may appear generally intact, but a few tubes can perforate first. In operation, this often appears as a “sudden” water leak, gas leak, or unexpected pressure loss.

In reality, the failure has usually been developing over a long period beneath deposits or inside localized cold spots.

Common Dew Point Corrosion Indicators

Early identification can reduce maintenance costs and unplanned downtime.

Symptom Possible Cause
Brown, yellow, or dark sticky deposits Acidic condensate mixed with fly ash
Rapid fin deterioration Low wall temperature and acid attack
Tube leakage near cold-end sections Localized sulfuric acid corrosion
Increasing pressure drop Ash fouling and deposit buildup
Falling heat transfer performance Fouling, corrosion products, or blocked fin channels
Corrosion near welds or tube ends Local temperature difference and crevice corrosion

How to Prevent Dew Point Corrosion in Flue Gas Heat Exchangers

The most effective strategy is to keep the metal wall temperature above the acid dew point throughout normal operating conditions, especially during startup, shutdown, and low-load operation.

1. Increase Tube Wall Temperature

Methods include:

  • Installing an air preheater or steam coil air heater
  • Raising inlet water temperature
  • Using recirculation to prevent cold-end water temperatures from dropping too low
  • Applying staged heat exchanger design
  • Optimizing gas-side and water-side flow distribution
  • Adding a bypass system for low-load operation

2. Reduce the Acid Dew Point

Reducing sulfuric acid formation can lower corrosion risk.

Common approaches include:

  • Using lower-sulfur fuel
  • Controlling excess oxygen and combustion conditions
  • Reducing SO₃ generation
  • Installing flue gas desulfurization equipment before low-temperature heat recovery
  • Optimizing SCR and catalyst operation where applicable

3. Select Corrosion-Resistant Heat Exchanger Materials

Material selection is the second line of defense when temperature control alone is not enough.

Material or Protection Method Main Advantage Typical Application
ND steel Improved sulfuric acid dew point corrosion resistance Boiler economizers and air preheaters
Stainless steel Good corrosion resistance in acidic environments Severe cold-end zones
Enameled tubes Strong acid resistance and anti-fouling performance Low-temperature flue gas heat recovery
Coated carbon steel Lower cost with protective barrier Moderate-corrosion applications
Non-metallic heat exchanger materials Excellent acid resistance Highly corrosive gas cooling systems

4. Avoid Extended Low-Load Operation

Low-load operation is one of the highest-risk conditions for dew point corrosion. Flue gas temperatures and tube wall temperatures both decrease, making acid condensation more likely.

A properly designed bypass, recirculation loop, or temperature-control system can protect the heat exchanger during low-load, startup, and shutdown periods.

Design Considerations for Finned Tube Heat Exchangers

For a finned tube manufacturer, corrosion-resistant design should include more than material selection.

Important design factors include:

  • Maintaining adequate minimum wall temperature
  • Selecting proper fin spacing to reduce ash blockage
  • Using corrosion-resistant tube and fin materials
  • Improving weld quality and reducing crevice areas
  • Designing for easy online or offline cleaning
  • Preventing uneven flue gas distribution
  • Optimizing tube arrangement for drainage and deposit removal
  • Providing bypass protection for abnormal operating conditions

Conclusion

Dew point corrosion in flue gas heat exchangers follows a clear chain of events:

  1. Sulfur-containing fuel generates SO₂ and SO₃.
  2. SO₃ reacts with water vapor and creates sulfuric acid vapor.
  3. Tube wall temperature drops below the acid dew point.
  4. Acid condensate forms and captures fly ash.
  5. Acidic deposits create under-deposit corrosion and reduce heat transfer.
  6. Localized areas eventually perforate and cause leakage or equipment failure.

The core solution is straightforward: keep the heat exchanger wall temperature above the acid dew point. Corrosion-resistant materials, enamel coatings, and optimized finned tube designs provide essential additional protection, but temperature control remains the first priority.